3M 4941 3.25" X 36YD

Description
TAPE DBL COATED GRY 3 1/4"X 36YD
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4941 3.25" X 36YD Overview

TAPE DBL COATED GRY 3 1/4"X 36YD

3M 4941 3.25" X 36YD Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.042"(42 mils,1.067mm)
Thickness - base fabric, carrier0.0030"(3.0 mils,0.076mm)
width3.25"(82.55mm)3 1/4"
length108' (32.9m) 36 yards
colorgrey
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Last year, I completed the drawing of the 4-layer PCB board for the router (or should I say the wiring was completed). I hope you can give me some advice.
[i=s]This post was last edited by chen468859 on 2017-1-24 16:38[/i] It was my first time drawing a 4-layer board. I was confused at first glance at so many schematic diagrams and components after they...
chen468859 PCB Design
Smart Home Assistant
What I envisioned cannot be completed independently by myself and requires teamwork. I can be responsible for the peripheral hardware design....
xu__changhua DSP and ARM Processors
Ask a question about VS2005
I downloaded the code from the Internet, and when I opened it, the following error message appeared: There was a failure while initializing the Microsoft Visual SourceSafe source control provider. You...
sinoxia Embedded System
51 serial port communication (dual 51 communication), question about SM2 bit
The experiment of two-machine communication (serial port working in mode 1) was not smooth. I tried to transfer three data directly according to the routine in the textbook, but it was unsuccessful. (...
辛昕 51mcu
After compiling Quartus II 9.1, it was found that the resource usage was 0%
I connected the signals of each module I wrote, compiled, and did layout and routing. After completion, I found that the resource utilization in the report was 0%? But I used many FIFOs in it. What is...
eeleader-mcu FPGA/CPLD
[Espier FPGA VHDL Learning Post] Post 18 Type Conversion
[align=center][color=red][font=宋体][size=16.0pt]【[/size][/font][/color][color=red][size=16.0pt]Espier[/size][/color][color=black][size=16.0pt] [/size][/color][color=red][size=16.0pt]FPGA VHDL[/size][/c...
常见泽1 FPGA/CPLD

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 196  572  835  1044  2767  4  12  17  22  56 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号