EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4932 9" X 1.25"-10

Description
TAPE DBL COATED 9"X 1 1/4" 10/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4932 9" X 1.25"-10 Overview

TAPE DBL COATED 9"X 1 1/4" 10/PK

3M 4932 9" X 1.25"-10 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0250" (25 mil, 0.635mm)
Thickness - Adhesive0.0220"(22.0 mils,0.559mm)
Thickness - base fabric, carrier0.0030"(3.0 mils,0.076mm)
width9.00"(228.60mm)
length1.25"(31.75mm)1 1/4"
colorWhite
use-
temperature range160°F (71°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
A simple way to implement TCP/IP protocol on ARM logic
With the continuous expansion of the application scope of embedded systems and the increasing popularity of network applications, more and more embedded systems need to support network functions. TCP/...
eeleader Microcontroller MCU
Effect of shear stress on iron loss of grain-oriented silicon steel sheets
Effect of shear stress on iron loss of grain-oriented silicon steel sheets Effect of scissional stress on loss of grain-oriented silicon steel sheetAs we all know, grain-oriented silicon steel sheets ...
fighting Analog electronics
In Verilog HDL, since while, repeat, and forever statements cannot be synthesized, what is their use?
Can anyone lend a hand? I am a novice and I really don't understand: In Verilog HDL, since while, repeat, and forever statements cannot be synthesized, what are they for? Also, I want to write a small...
pengwenxue FPGA/CPLD
How to modify component parameters in WEBENCH design?
[i=s]This post was last edited by dontium on 2014-6-30 18:10[/i] In the power supply--DCDC design of WEBENCH, when you open the circuit diagram, as shown in the figure, it prompts you to click to modi...
dontium Analogue and Mixed Signal
A trillion times, who cares?
[size=5][b]I saw a product news today - Fujitsu Semiconductor launches 1Mb FRAM memory device that can be erased and written 1 trillion times. 1 trillion times, 1Mb... very strong contrasting data. We...
frankuly RF/Wirelessly
CPU chip testing technical information
CPU chip testing technology...
环境试验箱 Domestic Chip Exchange

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1677  979  2276  1  2656  34  20  46  1  54 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号