EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4910 CIRCLE-0.625"-2000

Description
TAPE DBL COATED 5/8" DIA 2000/RL
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4910 CIRCLE-0.625"-2000 Overview

TAPE DBL COATED 5/8" DIA 2000/RL

3M 4910 CIRCLE-0.625"-2000 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierpolyethylene film
thickness0.0400"(40.0 mils,1.016mm)
Thickness - Adhesive0.0350"(35.0 mils,0.889mm)
Thickness - base fabric, carrier0.0050"(5.0 mils,0.127mm)
width0.63" (16.00mm) 5/8" diameter
length-
colortransparent
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
A new interpretation of the principle of integral circuits: the transformation of amplifiers and capacitors
I saw a very good article on the Internet about integral circuits and how to understand the role of capacitors. It can be used as a method to qualitatively study integral circuits. I reprinted it for ...
fish001 Energy Infrastructure?
A paradise for programmer friends——Programmer Club
There is a programmers club that organizes lectures and discussions on the latest technologies on weekends, as well as ball games and cultural activities. It's pretty good. The National Day prize-givi...
huangl53 Embedded System
Serial port help
Question: Why are the messages sent and received different? For example, if I send 00, I receive 80, etc. The procedure is as follows:#includereg52.hvoid init(){EA=1; ES=1; TMOD=0x20; SCON=0x50; TH1=0...
张丽山 51mcu
ucos task stack
Each task has its own stack, which must be declared as OS_STK type and consists of continuous memory space. Stack space can be allocated statically or dynamically. The first half of the sentence makes...
sxy4517 Real-time operating system RTOS
To go or to stay, about technology! Confused!
Hello everyone, I haven't posted on eeworld for a long time! I have seen many X-cows in the forum! The posts they posted said "People with low education should not develop in the embedded industry". I...
zhuxl Robotics Development
The program is typed and output to .txt, but it cannot be burned into the chip
[i=s]This post was last edited by chi80929 on 2015-8-31 16:00[/i] I need help from experts. I wrote a simple program to try out my new board, but it keeps saying "could not open port". I can't burn it...
chi80929 Microcontroller MCU

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 406  141  1497  555  1859  9  3  31  12  38 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号