EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4951 0.75" X 2"-5

Description
TAPE DBL COAT WHT 3/4"X 2" 5/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4951 0.75" X 2"-5 Overview

TAPE DBL COAT WHT 3/4"X 2" 5/PK

3M 4951 0.75" X 2"-5 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width0.75"(19.05mm)3/4"
length2.00"(50.80mm)
colorWhite
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Serial communication mode
Please help me explain the meaning of the following parameters. I don't understand the meaning of the last two parameters. Baud rate 115200, N, 8, 0, 1...
ccxida Embedded System
Experience in debugging Ethernet half-duplex of GD32F450
I guess many people have almost forgotten about Ethernet half-duplex. Believe it or not, we have recently started using Ethernet half-duplex. In the final analysis, it is to save costs. Due to the sim...
心☆野 GD32 MCU
God, please help me
Is there any reliable solution to make an LC voltage-controlled oscillator? It is definitely possible, with a frequency range of 10k to 40kHZ, and I am not afraid to spend money...
顽皮小孩儿 Electronics Design Contest
DAO layer, Service layer, Controller layer, View layer collaborative working mechanism
[size=5]DAO layer: The DAO layer is mainly responsible for the work of the data persistence layer. Some tasks responsible for communicating with the database are encapsulated here. The design of the D...
Jacktang DSP and ARM Processors
#AugustOriginal# Understanding the logic unit of Altera V series devices
[i=s]This post was last edited by coyoo on 2015-8-14 16:50[/i] Altera's latest main push is the Cyclone V, Arria V GX and high-end Stratix V series. Compared with the previous series of products, in a...
coyoo DIY/Open Source Hardware
Speak your opinion and have a different Tanabata match~
[size=4][color=#ff8c00]Hello, everyone. Another Chinese Valentine's Day is coming. Engineers, are you surrounded by pink hearts? [/color][/size] [size=4][color=#483d8b]Every year on Chinese Valentine'...
okhxyyo Suggestions & Announcements

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1535  2437  2248  478  2074  31  50  46  10  42 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号