EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4943F 4" X 7"-6

Description
TAPE DBL COAT GRAY 4"X 7" 6/PACK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4943F 4" X 7"-6 Overview

TAPE DBL COAT GRAY 4"X 7" 6/PACK

3M 4943F 4" X 7"-6 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width4.00"(101.60mm)
length7.00"(177.80mm)
colorgrey
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
When using 430 MCU as ADC, only channel 0 is OK in single channel measurement, while other channels are not accurate. What is the problem?
RT:430 MCU is used as ADC. Only channel 0 is OK in single channel measurement. Other channels are not accurate. What is the problem? It is really a headache. Only channel 0 is accurate. Any other chan...
qq4988 Microcontroller MCU
Problems sending MMS
Hello everyone, I am now using HTTP1.1 protocol to send MMS, I just need to combine an HTTP header and MMS PDU. But now the HTTP header always replies with 400 error, and returns 200OK without adding ...
HHY55 Embedded System
The evil FSMC driving LCD (ILI9341 controller) detailed explanation
[b][url=http://www.amobbs.com/thread-5493735-1-1.html][color=#0066cc]The evil FSMC driving LCD (ILI9341 controller) detailed explanation[/color][/url] Wildfire dedication[/b]...
wangbin65530 stm32/stm8
Project Navigator Window
I accidentally made the project navigator window float, and I can't accept it because of my obsessive-compulsive disorder, but I don't know how to change it back. I urgently need someone to teach me h...
zhenpeng25 FPGA/CPLD
Ask a question + CC Debugger Firmware Update
[i=s]This post was last edited by tianshuihu on 2014-3-11 10:50[/i] When I opened SmartRF Flash Programmer, it prompted that a new version of the firmware was available, so I updated it and clicked th...
tianshuihu Wireless Connectivity
MSP430 and STM32PK, which one has a better price-performance ratio?
I am a beginner and I am confused whether to learn MSP430 or STM32? In your study or work, do you use MSP430 more or STM32 more? Why would you choose MSP430 or STM32? Which one is more cost-effective?...
AnyMax Microcontroller MCU

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1585  1847  103  1570  975  32  38  3  20  28 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号