EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4930 1" X 3"-100

Description
TAPE DBL COATED WHT 1"X 3" 100PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4930 1" X 3"-100 Overview

TAPE DBL COATED WHT 1"X 3" 100PK

3M 4930 1" X 3"-100 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0250" (25 mil, 0.635mm)
Thickness - Adhesive-
Thickness - base fabric, carrier-
width1.00"(25.40mm)
length3.00"(76.20mm)
colorWhite
useUniversal
temperature range200°F(93°C)
Shelf life start dateShip date
shelf life24 months
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
[AN-758 Application Note] Using ADE7753 to generate reactive energy pulse output
Introduction: This application note describes how to use the reactive energy readings of the ADE7753 to generate a pulse output....
EEWORLD社区 ADI Reference Circuit
Fujitsu FRAM Experience Submission
The efficiency of applying for Fujitsu's FRAM is unexpectedly high. In the past, it usually took more than ten days to apply for samples from other manufacturers. When applying for a few chips worth a...
startcortexmo Integrated technical exchanges
TB CLLD Question
What is the function of the CLLD bit in the TB timer register? I don't understand~...
zzbaizhi Microcontroller MCU
Make Image Problem
After the modification, the build passed, but an error occurred in make image: Error: Failed to allocate memory in Data object Error: Failed reading comment structurenk.exe Fatal error hit, exiting......
huleisheng Embedded System
timerA interrupt problem!
//-------------------------------------------------------------------------void main(void){WDTCTL = WDTPW + WDTHOLD; // Stop watchdog timerDCOCTL=0xe0; //High frequency state, DCO=7BCSCTL1=0xb7; //Osc...
houge Microcontroller MCU
【CN0078】Using audio codec and microphone to build a stereo digital microphone input
The circuit shown in Figure 1 allows up to two iMEMS digital microphones to interface with an audio codec. The ADMP421 includes a MEMS microphone element, an output amplifier, and a fourth-order Σ-Δ m...
EEWORLD社区 ADI Reference Circuit

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 466  46  2086  2828  2845  10  1  42  57  58 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号