3M 4959 8" X 1.25"-10

Description
TAPE DBL COATED 8"X 1 1/4" 10/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4959 8" X 1.25"-10 Overview

TAPE DBL COATED 8"X 1 1/4" 10/PK

3M 4959 8" X 1.25"-10 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.1200"(120.0 mils,3.048mm)
Thickness - Adhesive0.1180"(118.0 mils,2.997mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width8.00"(203.20mm)
length1.25"(31.75mm)1 1/4"
colorWhite
use-
temperature range300°F (149°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Look forward to experiencing advanced power management technology - 0.25 micron high voltage process technology
The BCD (Bipolar-CMOS-DMOS) process technology, a 0.25-micron high-voltage process technology, developed by TSMC and German Dialog Semiconductor, can effectively integrate various high-voltage functio...
雪山飞狐 Power technology
Migrating the work environment from Redhat 9 to Fedora Core 5
I have been developing embedded software under RedHat 9 Linux, usually using C language and the built-in KDevelop. Now I have moved to Fedora Core 5. The issues involved in the migration are:Convert t...
yytzc Embedded System
The company wants to terminate the labor contract, and provide consultation on severance compensation
[i=s]This post was last edited by sanhuasr on 2021-6-20 08:45[/i]I complained about project management in front of my boss in the work group, and then I was kicked out. Then my computer account was su...
sanhuasr Talking
Using DSP timer to realize square wave output
1. Initialize the timer value to half a period value.ConfigCpuTimer(CpuTimer2, 100, 10); StartCpuTimer2();2. The interrupt procedure is as follows: interrupt void CpuTim2Int(void) { Uint32 i; if (Stat...
xiaoruo DSP and ARM Processors
PCB motherboard loading and unloading automation
PCBs used in mobile phone factories need to be fixed on the patch fixture before entering the patch machine. At present, our department uses manual operation to take the motherboard and place it on th...
心仪 Industrial Control Electronics
8-way temperature test, parameter modification and writing into memory
Here are two about 8-way temperature test, parameter modification (upper limit temperature, lower limit temperature) written into the memory, share with you, hope you can find out the mistakes or opti...
15075039ZQ MCU

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2229  1760  224  570  1276  45  36  5  12  26 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号