EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4949 1" X 4"-100

Description
TAPE DBL COAT BLK 1"X 4" 100/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4949 1" X 4"-100 Overview

TAPE DBL COAT BLK 1"X 4" 100/PK

3M 4949 1" X 4"-100 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width1.00"(25.40mm)
length4.00"(101.60mm)
colorblack
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
I don’t know what went wrong with the program, but the LCD shows nothing.
[color=#ff0000]This is a program, please help me[/color] #include #include#define SYSCLK 24500000 #define uchar unsigned char #define uint unsigned int sfr16 TMR2RL = 0xca; // Timer2 reload value sfr1...
wtkkl123 51mcu
Compilation help, thank you
When using assembly instructions, the error "PC offset out of range" occurs when using the jump instruction JEQ. What instruction can be used instead of JEQ to achieve large-range addressing?...
abab0908 NXP MCU
WinCE5.0 simulator
Why is there no WinCE 5.0 simulator in VS2005? Where can I download it? Note: It is "WinCE 5.0 simulator", not "Pocket PC simulator" or "Smart Phone simulator"...
caosc Embedded System
Application Engineer Q&A — 30
...
EEWORLD社区 ADI Reference Circuit
Digital IC Power Supply Noise Suppression and Decoupling Application Note
Continued from the previous article~~~~~ Continue the decoupling/bypass journey~~~~~~~· This is Murata's decoupling application manual, which is quite comprehensive, explaining decoupling applications...
nathanzhang Energy Infrastructure?
An unexpected surprise! Postgraduate entrance examination + employment!
Special issue for postgraduate entrance examination and employment Postgraduateentrance examination process + postgraduate entrance examination experience + talent recruitment fair + salary negotiatio...
gaoxiao Microcontroller MCU

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1843  1116  709  583  2518  38  23  15  12  51 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号