EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4949 0.75" X 1.25"-25

Description
TAPE DBL COAT 3/4"X 1 1/4" 25/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4949 0.75" X 1.25"-25 Overview

TAPE DBL COAT 3/4"X 1 1/4" 25/PK

3M 4949 0.75" X 1.25"-25 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width0.75"(19.05mm)3/4"
length1.25"(31.75mm)1 1/4"
colorblack
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
How is the dead time of STM32 timer 1 calculated? TIM1_BDTR
How is the dead time of STM32 timer 1 calculated? TIM1_BDTR. The dead zone is described on page 249 of the STM32F10XX data sheet as follows. UTG[7:0]: Dead-time generator setup Bits 7:0 These bits def...
yuke30 stm32/stm8
PCI BIOS development issues
Hello, I'm developing PCI BIOS recently. There is no problem with the basic functions, but I can't return to the motherboard BIOS that called it after executing PCI BIOS. I checked some information, b...
wzqqz Embedded System
The FatFs file system of LPC1114 is unstable! ! !
I have successfully transplanted the routines for reading and writing FATFS on LPC1114. The reading and writing functions can be realized, but when reading and writing for a long time (almost half a d...
wyl7525 NXP MCU
Jinan High-tech Zone Integrated Circuit Company Recruitment
Software Engineer (2 persons) Main responsibilities: 1. Engage in the development of wireless sensor network application software 2. Carry out detailed design of submodules, code writing, unit testing...
uwb11n Recruitment
X-NUCLEO-IKS02A1 Industrial Sensor Evaluation Board Data
An industrial sensor development board launched by ST, equipped with an Arduino UNO R3 connector, can be directly connected to the STM32 Nucleo development board or other development boards that suppo...
littleshrimp MEMS sensors
Can you please tell me what is reentrancy in wdm? Or what situations lead to reentrancy?
Can you please tell me what is reentrancy in wdm? Or what situations lead to reentrancy?...
lg7412374123 Embedded System

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2090  507  2547  453  139  43  11  52  10  3 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号