EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4943F 0.5" X 8"-15

Description
TAPE DBL COAT GRY 1/2"X 8" 15/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4943F 0.5" X 8"-15 Overview

TAPE DBL COAT GRY 1/2"X 8" 15/PK

3M 4943F 0.5" X 8"-15 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width0.50"(12.70mm)1/2"
length8.00"(203.20mm)
colorgrey
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Is there anything that can sense the slight vibration when the solenoid valve is actuated?
I am planning to implement an application where the solenoid valve is buried deep inside. Since the valve may fail sometimes, I hope to get information about whether the valve has been actuated after ...
天涯海角sr Analog electronics
Urgently need experts familiar with uCOS, with compensation
A project in my company is similar to a handheld GPS. The hardware environment is basically an FPGA development board, Altera's 2C series, using a Nios soft-core CPU. The development environment is Ni...
zyandll123 Real-time operating system RTOS
【Paper】Design of wireless infrared anti-theft alarm system based on zigbee
Abstract: Combining the two hot topics of infrared anti-theft alarm and ZigBee technology, the hardware design and software development of the wireless infrared anti-theft alarm system based on ZigBee...
linjiang Download Centre
Ask about electronic locks
I want to use 51 to make an electronic lock, but I don't know how to do it. I hope you can give me some ideas, and it would be best if you can attach a circuit diagram or something....
roseswing Mobile and portable
Help on ADN8834 burning out
The phenomenon encountered is that after powering on, ADN8834 works normally at first, and then after powering on again, it is found that the supply current increases and the voltage is pulled down. A...
Anjiang Analog electronics
In my personal experience, there are some common misunderstandings in wireless selection:
In my personal experience, there are some common misunderstandings in wireless selection: 1. Communication rate. For example, many companies advertise that the rate of NRF2401 is 1MBPS. However, in fa...
hygk Robotics Development

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 22  670  1374  2888  2370  1  14  28  59  48 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号