CHP1/8-1003093F7LF

Description
Fixed Resistor, Metal Glaze/thick Film, 0.25W, 309000ohm, 200V, 1% +/-Tol, 100ppm/Cel, Surface Mount, 1206, ROHS COMPLIANT
CategoryPassive components    The resistor   
File Size382KB,3 Pages
ManufacturerTT Electronics plc
Websitehttp://www.ttelectronics.com/
Environmental Compliance  
Download Datasheet Parametric View All

CHP1/8-1003093F7LF Overview

Fixed Resistor, Metal Glaze/thick Film, 0.25W, 309000ohm, 200V, 1% +/-Tol, 100ppm/Cel, Surface Mount, 1206, ROHS COMPLIANT

CHP1/8-1003093F7LF Parametric

Parameter NameAttribute value
Is it lead-free?Lead free
Is it Rohs certified?conform to
MakerTT Electronics plc
package instructionMELF, 1206
Reach Compliance Codecompliant
ECCN codeEAR99
structureCylindrical
JESD-609 codee1
Installation featuresSURFACE MOUNT
Number of terminals2
Maximum operating temperature150 °C
Minimum operating temperature-55 °C
Package diameter1.45 mm
Package length3.25 mm
Package shapeCYLINDRICAL PACKAGE
Package formMELF
method of packingTR, 7 INCH
Rated power dissipation(P)0.25 W
Rated temperature70 °C
resistance309000 Ω
Resistor typeFIXED RESISTOR
seriesCHP
size code1206
surface mountYES
technologyMETAL GLAZE/THICK FILM
Temperature Coefficient100 ppm/°C
Terminal surfaceTin/Silver/Copper (Sn96.0Ag3.5Cu0.5)
Terminal shapeWRAPAROUND
Tolerance1%
Operating Voltage200 V
Cylindrical High Power
Surface Mount Metal Glaze™
CHP Series
·
Cylindrical High Power
Up to 2 watts
·
Surface Mount Metal Glaze
TM
Up to 1000 volts
·
0.2 ohm to 2.2 megohm range
·
Up to 2 watts
RoHS-compliant version available
·
Up to 1000 volts
150°C maximum operating temperature
0.2 ohm to 2.2 megohm range
RoHS-compliant version available
150°C maximum operating temperature
CHP
Metal Glaze™
thick fi lm element
fi red at 1000°C
to solid ceramic
Metal Glaze
TM
thick film element
fired at 1000°C
to solid ceramic
Solder over
nickel barrier
Solder over
nickel barrier
High
temperature
dielectric
coating
High
temperature
dielectric
coating
Electrical Data
IRC
Type
Indus-
try
Foot-
print
1206
Size
Code1
Maximum
Power Rating
Working
Voltage²
Maximum
Voltage
Resistance
Range (ohms)³
0.1 to 0.99
CHP 1/8
B&C
1/4W @ 70°C
200
400
1.0 to 1.0 M
20 to 348K
CHP 1/2
2010
D&E
1/2W @ 70°C
300
600
0.1 to 0.99
1.0 to 348K
0.1 to 0.99
CHP 1
2512
F
1W @ 70°C
350
700
1.0 to 2.21M
20 to 348K
CHP 2
3610
H
2W @ 25°C
1.33W @ 70°C
500
1000
0.2 to 0.99
1.0 to 2.21M
²Not to exceed
P x R
Product
Category
Low Range
Standard
Tight Tolerance
Low Range
Standard
Low Range
Standard
Tight Tolerance
Low Range
Standard
Tolerance
(±%)³
1, 2, 5
1, 2, 5
0.25, 0.5
1, 2, 5
1, 2, 5
1, 2, 5
1, 2, 5
0.25, 0.5
1, 2, 5
1, 2, 5
TCR
(ppm/°C)³
100
50, 100
50, 100
100
50, 100
100
50, 100
50, 100
100
50, 100
¹See pages 2 & 3 for product dimensions, recommended solder pads, and standard packaging.
³Consult factory for tighter TCR, tolerance, or resistance values.
Environmental Data
Characteristics
teristics
Charac
Thermal Shock
Temperature Coefficient
Thermal Shock
Low Temperature Operation
Maximum
m Change
Maximu
Change
±0.25% +.01 Ω
As specified
±0.5% + 0.01 ohm
±0.25% +.01 Ω
±0.25% + 0.01 ohm
±0.5% +.01 Ω
Test Method
MIL-PRF-55342H, §4.8.3
Test Method
MIL-R-55342H Par 3.16 (-55°C +
+150°C / -65°C)
(MIL-STD-202, Method 107G:
125°C)
MIL-PRF-55342H, §4.8.5
MIL-R-55342H Par 3.9 (-65°C + 150°C, 5 cycles)
(-65°C)
MIL-R-55342H Par 3.11 (-65°C @ working voltage)
MIL-R-55342H Par 3.12
2.5 x
P x R
for 5 seconds
MIL-PRF-55342H, §4.8.7
MIL-R-55342H Par 3.13 (-150°C for 100 hours)
MIL-R-55342H Par 3.14.2 (
Reflow soldered to board at 260°C for 10 seconds
)
MIL-PRF-55342H, §4.8.8.2
Short Time Overload
Low Temperature Operation
Short Time Overload
High Temperature Exposure
Resistance to Bonding
Exposure
±1%
+ 0.01 ohm
±0.5%
for R>100KΩ
±1% for R>100K ohm
±0.5% + 0.01 ohm
±0.25% + 0.01 ohm
MIL-PRF-55342H, §4.8.6
(150°C x 100 Hours)
Resistance to Bonding Exposure
Moisture Resistance
Solderability
High Temperature Exposure
±0.5% +.01 Ω
±0.25% +.01 Ω
±0.5% +.01 Ω
As specified
MIL-PRF-55342H, §4.8.8.2
95% minimum coverage
±0.5% + 0.01 ohm
Temperature Coefficient
Life Test
Resistance
Moisture
Life Test
Solderability
Terminal Adhesion Strength
MIL-PRF-55342H, §4.8.10
(MIL-STD-202, Method 304)
MIL-R-55342H Par 3.18 (10 cycles, total 240 hours)
MIL-R-55342H Par 3.15 (2000 hours at 70°C intermittent)
(MIL-STD-202, Method 108A: 2000 Hours @ 70°C)
1200 gram push from underside of mounted chip for 60 seconds
(MIL-STD-202, Method 208H)
MIL-STD-202, Method 208 (245°C for 5 seconds)
(MIL-STD-202, Method 106G)
±1%
+ 0.01
±0.5%
+.01 Ω
ohm
±1% +
minimum coverage
95%
0.01 ohm
no mechanical damage
MIL-PRF-55342H, §4.8.11
MIL-PRF-55342H, §4.8.12
±1% +.01 Ω
IRC – defined
Chip mounted in center of 90mm long board, deflected 1mm so as to
Terminal Adhesion Strength (push)
±1% + 0.01 ohm
(no mechanical damage)
exert pull on chip contacts for 5 seconds
1200 gram push from underside of mounted device for 60 sec
no mechanical damage
IRC-defined
±1% +.01 Ω
General Note
Device mounted in center of 90mm long board, deflected 1 mm to exert
Terminal Adhesion Strength (flex)
cation without notice or liability.
IRC reserves the right to make changes in product specifi
(no mechanical damage)
All information is subject to IRC’s own data and is considered accurate at time of going to print.
pull on contacts for 5 seconds
A subsidiary of
© IRC Wire and Film Technologies Division
General Note
Telephone:
Facsimile:
Website: www.irctt.com
rpus Christi Te
TT electronics plc
ries Issue March
TT electronics reserves the right to make changes in product specification without notice or liability.
All information is subject to TT electronics’ own data and is considered accurate at time of going to print.
www.bitechnologies.com www.irctt.com www.welwyn-tt.com
© TT electronics plc
09.12
2005 Network World Conference - Building Adaptive Networks and Promoting the Development of Ethernet
From its earliest appearance to now, IT architecture has penetrated into the information processing process of various enterprises and institutions. In fact, it has gone through several stages. I will...
liudong2008lldd RF/Wirelessly
Zigbee debugging problem, please help
How to solve the problem as shown in the picture...
旧而久之 RF/Wirelessly
S3C6410 Memory Map Memory Map (1)
S3C6410 chip secrets 4 S3C6410 memory map memory mapMemory Map Memory MapS3C6410 supports 32-bit physical address domains, and these address domains are divided into two parts, one for storage and the...
haoboy ARM Technology
ATMEL has released a web version peripheral selection code generator similar to CUBE, but the web version
[i=s]This post was last edited by damiaa on 2015-10-8 09:40[/i] ATMEL has released a web version of the peripheral selection code generator similar to CUBE, but the web version [url=http://start.atmel...
damiaa Microchip MCU
Transformer Design Example
eeworldpostqq...
blink Power technology
DIY Gloldensea_FPGA
I recently looked up some information and designed a Cylone2 FPGA board based on some good solutions from experts. I will upload the information after I finish organizing it. How can I upload it if I ...
鑫海宝贝 FPGA/CPLD

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2788  1027  679  1089  1511  57  21  14  22  31 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号