EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4952 4" X 4"-10

Description
TAPE DBL COATED WHT 4"X 4" 10/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4952 4" X 4"-10 Overview

TAPE DBL COATED WHT 4"X 4" 10/PK

3M 4952 4" X 4"-10 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.042"(42 mils,1.067mm)
Thickness - base fabric, carrier0.0030"(3.0 mils,0.076mm)
width4.00"(101.60mm)
length4.00"(101.60mm)
colorWhite
use-
temperature range160°F (71°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Please help me with the ACMD41 argument when initializing the SDHC card
When writing data to the SD card via 430, the SD card can be used. However, during the initialization of the SDHC card, the response of CMD0 is correct, but the response of ACMD41 is always 0x01. Is t...
nothingo Microcontroller MCU
Linux/UNIX System Programming Manual (Volumes 1 and 2)
"Linux/UNIX System Programming Handbook (Volumes 1 and 2)" is an authoritative book introducing the programming interface between Linux and UNIX. Michael Kerrisk, a senior Linux programming expert, de...
arui1999 Download Centre
Inductive Sensing: Designing a Stacked Coil for Switching Applications with WEBENCH Coil Designer
[align=left][color=#000]In a previous blog post [color=rgb(205, 23, 31)][url=http://e2e.ti.com/blogs_/b/analogwire/archive/2015/08/19/inductive-sensing-how-to-design-an-inductive-sensor-with-the-new-w...
maylove Analogue and Mixed Signal
The difference between VC and EVC
What is the difference between VC and EVC?...
54288519 Embedded System
uCOS-ii for S3c44b0x
I have a lot of uCOS-II collections that I will upload one after another. If anyone has Nucleus, please send it to me....
jinpost Real-time operating system RTOS
Difficulty in learning the principles and applications of microcomputer systems
I don't know how to program the 8237A, 8259A, 8253-PIT, 8255A, 8250, and 8251A chips mentioned in the book. Do you have any good suggestions to help me master them? Are there any good materials?...
flamingo315 Embedded System

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2123  99  600  464  438  43  2  13  10  9 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号