EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4949 7" X 8"-2

Description
TAPE DBL COAT BLK 7"X 8" 2/PACK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4949 7" X 8"-2 Overview

TAPE DBL COAT BLK 7"X 8" 2/PACK

3M 4949 7" X 8"-2 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width7.00"(177.80mm)
length8.00"(203.20mm)
colorblack
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
FPGA Design Practice (Logic)
FPGA Design Practice (Logic) is aimed at the vast number of FPGA/CPLD beginners. It explains FPGA/CPLD and related basic knowledge from scratch, and uses a motherboard-based learning kit that supports...
arui1999 Download Centre
SIMterix-Simplies~4~ Verilog
In the case of mixed integer and analog systems, simulation can only simulate Verilog or analog. If the digital part has only output, it is OK, just edit the voltage source and import the waveform fil...
xutong Analog electronics
CCS Error
DEBUG: Error 2863: The control PushButton2 on dialog Installation_Type_Dialog needs the icon TypicalInstall.bmp in size 48x48, but that size is not available. Loading the first available sizeInternal ...
feiyun DSP and ARM Processors
When the CEdit control is deleted by pressing the back key under EVC4.0\wince5, the content of CEdit is not updated
The cursor has moved over, but the string is still displayed there. It is updated only when the line is deleted. If you enter again, it will overlap with the previous word. And this problem only occur...
zhangheng Embedded System
After IAR compiles and downloads the code, how do I know the total length of the code and where the address is from and to?
Is there any automatically generated file that I can look at directly?Thanks!...
jsglf Microcontroller MCU
Is it possible to add a count loop in the combinational logic of a three-stage state machine?
Assuming the clock cycle is 40ns, the state changes of my sequential circuit are about 80ns, 160ns, 160ns, 40ns. In a state, it relies on counting loops to stay in this state until the loop count meet...
lvben5d FPGA/CPLD

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1273  395  2395  1565  1567  26  8  49  32  50 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号