EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4930 1.5" X 7"-12

Description
TAPE DBL COATED 1 1/2"X 7" 12/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4930 1.5" X 7"-12 Overview

TAPE DBL COATED 1 1/2"X 7" 12/PK

3M 4930 1.5" X 7"-12 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0250" (25 mil, 0.635mm)
Thickness - Adhesive0.0220"(22.0 mils,0.559mm)
Thickness - base fabric, carrier0.0030"(3.0 mils,0.076mm)
width1.50"(38.10mm)1 1/2"
length7.00"(177.80mm)
colorWhite
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
What the hell, PCB routing also depends on the shape? !
Original article by Mr. Gaosu, the self-media of Yibo Technology | Huang GangAs the old saying goes: A gentleman loves a beautiful lady. If you are asked to choose between a tall and thin lady and a s...
yvonneGan PCB Design
Power supply design tip 2: Harnessing noisy power supplies
[align=left][color=rgb(85, 85, 85)]Noise-free power supplies are not designed by accident. A good power supply layout is designed to minimize experimentation time. Minutes or even hours spent carefull...
莫妮卡 Analogue and Mixed Signal
[Chuanglong Technology Allwinner A40i Development Board] Building a development environment and Qt development experience based on virtual machine images
Preface The installation based on the SDK file on the CD is cumbersome, and various dependencies are installed, and the build may fail. So in order to avoid wasting too much time on the installation e...
qinyunti Domestic Chip Exchange
SI4432 Direct Mode
Is there any expert who has done Si4432 direct mode and can give me some guidance? I use si4432 for serial port transparent transmission. If I use FIFO mode, when the serial port rate reaches 9600bps,...
morewater RF/Wirelessly
Headhunting position: Engineers to the United States! Contact 13381085719 13381085771 Mr. Liu
Headhunting position: Engineers to the United States! Contact 13381085719 13381085771 Mr. Liu...
张肖肖 Embedded System
A newbie asks a question about data, idata, and xdata
Because some relatively large idata type global variables are defined in the program, the 256 bytes of RAM are not enough. I have selected the small mode. Without considering optimization, can I chang...
a8461813 MCU

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2585  2809  2310  1403  320  53  57  47  29  7 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号