EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4949 1.5" X 7"-10

Description
TAPE DBL COATED 1 1/2"X 7" 10/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4949 1.5" X 7"-10 Overview

TAPE DBL COATED 1 1/2"X 7" 10/PK

3M 4949 1.5" X 7"-10 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width1.50"(38.10mm)1 1/2"
length7.00"(177.80mm)
colorblack
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
New preferential policies for the semiconductor industry
New national policy to support semiconductor industry is expected to be released in the second half of the year 2006-7-7Li Ke, director of the China Semiconductor Industry Association, revealed that t...
ehk RF/Wirelessly
Function entry address problem
How to write the already compiled C51 program into the specified memory address?...
nlinger Embedded System
Um... there seems to be some problems with the layout of some pages?
For example, the following...It feels like the webpage is not finished yet... not very beautifulIn this case, there is no problem with some sections, but when there is too much information in the sect...
anqi90 Suggestions & Announcements
Several important questions about Zigbee
Hello everyone, I am a zigbee newbie, but in the process of studying bdbs, there are a few questions that I have not been able to understand: 1. Zigbee supports mesh, and mesh expands the network rang...
gymiicmc RF/Wirelessly
Great Gods, this is a paid post, I hope you can help me
I hope to use vs2010 and opencv2.4.10 to make a target tracking system on PC. The algorithm is at [url]http://blog.csdn.net/bcbobo21cn/article/details/50894736[/url] If you can help, please contact 79...
JerryHetty Programming Basics
Lattice dual port RAM read and write
Why can't I write data into the lattice dual-port RAM?...
lxglovehome FPGA/CPLD

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 2829  713  2688  176  1486  57  15  55  4  30 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号