3M 4951 5" X 9"-5

Description
TAPE DBL COAT WHT 5"X 9" 5/PACK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4951 5" X 9"-5 Overview

TAPE DBL COAT WHT 5"X 9" 5/PACK

3M 4951 5" X 9"-5 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width5.00"(127.00mm)
length9.00"(228.60mm)
colorWhite
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Programming Skills Cheatsheets for College Students
[p=28, null, left]I went to attend [color=inherit][font=inherit][url=https://kktix.com/events/happydesigner-mini-5]HappyDeisgner Mini #5[/url][ yesterday /font][/color] I heard Caesar Chi telling the ...
qinkaiabc Programming Basics
MOTOROLA M68HCO5 series microcontrollers and their application fundamentals
Title: Motorola M68HCO5 Series Microcontrollers and Their Application Basics Author: Gang Hanbing et al. Publisher: Beijing University of Aeronautics and Astronautics Press Publication Date: November ...
wzt MCU
Please help me, esp8266 firmware update problem
This is what happened after updating the firmware. Is there a solution?...
goldmira MicroPython Open Source section
How to make the registry take effect immediately under wince?
As the title says! Is it possible to make the registry take effect immediately without restarting?...
lz36000 Embedded System
How to burn cg's 2812
I use cg's 2812, but the program cannot be written successfully. It always shows "unload failed". But I have never locked the chip. It is a new chip. Has anyone done this before? Can you tell me the d...
beijilang5 Microcontroller MCU
Smart Micro MM32F0270 timer DMA mode output PWM
For controlling stepper motors, the most important control parameters are the number and frequency of pulses. The combination of the two can achieve the required motor acceleration and deceleration cu...
火辣西米秀 Domestic Chip Exchange

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1165  1228  2318  687  1849  24  25  47  14  38 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号