3M 4930 1" X 8"-12

Description
TAPE DBL COATED WHT 1"X 8" 12/PK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4930 1" X 8"-12 Overview

TAPE DBL COATED WHT 1"X 8" 12/PK

3M 4930 1" X 8"-12 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPaper
thickness0.0250" (25 mil, 0.635mm)
Thickness - Adhesive0.0220"(22.0 mils,0.559mm)
Thickness - base fabric, carrier0.0030"(3.0 mils,0.076mm)
width1.00"(25.40mm)
length8.00"(203.20mm)
colorWhite
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Can someone please help me with these questions? I want the answers!
[font=微软雅黑][size=5]1.After the program written in CCS is downloaded to the MSP430F5529 microcontroller, is the program saved in RAM or FLASH? What is the basis for judgment? [/size][/font] [font=微软雅黑]...
阿蒙放过谁 51mcu
Which brother can help me come up with a plan?
For my graduation project, I have an operating rod with several degrees of freedom, such as up and down, left and right, inside and outside, and axial rotation, relative to a hole on a fixed plane. Ca...
qtworry Sensor
How to add a menu to a program with only one modal dialog box
My program has only one modal dialog box, and no createwindow main window. I want to add a menu to the dialog box, which is the "About" option in the lower right corner. I copied and pasted the defaul...
haian_bch Embedded System
TI is really interesting, and they also gave me a lucky draw tool
Let's have a family portrait firstIs this lottery tool familiar?internalOne 12002 module, one 10501 module, one 12001 chip and one 23610 chip10501 is so small! 23610 is scary, what kind of power suppl...
柳叶舟 Analogue and Mixed Signal
Changes in Linux 2.6 interrupt registration
irqreturn_t int_interrupt(int irq,void * dev_id,struct pt_regs *regs); register interrupt function extern int __must_check request_irq(unsigned int, irq_handler_t handler,unsigned long, const char *, ...
ren364940161 Linux and Android
【National Technology N32G430】05 The page is initially displayed, system composition
05 The page is initially displayed, system composition In order to ensure that the tests are carried out in an orderly manner and displayed effectively, the page display is prepared before the test, s...
秦天qintian0303 Domestic Chip Exchange

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 1797  1636  842  1014  2753  37  33  17  21  56 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号