EEWORLDEEWORLDEEWORLD

Part Number

Search

3M 4949 1" X 3"-5

Description
TAPE DBL COAT BLK 1"X 3" 5/PACK
Categoryaccessories   
File Size156KB,6 Pages
Manufacturer3M
Websitehttp://3M.com/esd
Environmental Compliance
Download Datasheet Parametric View All

3M 4949 1" X 3"-5 Overview

TAPE DBL COAT BLK 1"X 3" 5/PACK

3M 4949 1" X 3"-5 Parametric

Parameter NameAttribute value
Tape typeDouble coated, double sided
Adhesiveacrylic acid
base fabric, carrierPolyester film
thickness0.0450"(45.0 mils,1.143mm)
Thickness - Adhesive0.0430"(43.0 mils,1.092mm)
Thickness - base fabric, carrier0.0020"(2.0 mils,0.051mm)
width1.00"(25.40mm)
length3.00"(76.20mm)
colorblack
use-
temperature range200°F (93°C) maximum
shelf life24 months
Shelf life start dateShip date
3
3M VHB Tape Durability
TM
TM
Technical Bulletin
Summary
August, 2018
This bulletin addresses the long-term durability of 3M™ VHB™ Tapes and
their ability to perform in certain types of demanding environments. This
will be addressed from a variety of view-points including chemical
composition, resistance to harsh environments, 3M and independent tests
for product durability, and certain applications where 3M™ VHB™ Tape
products have demonstrated excellent ability to perform in demanding
applications. Test results on moisture resistance, UL durability,
accelerated weathering, outdoor weathering, thermal cycling and fatigue
resistance will be discussed.
3M is a technological leader in acrylate pressure sensitive adhesive (PSA)
technology. 3M™ VHB™ Tapes represent examples of 3M’s proprietary,
state-of-the-art chemistry. The long-term aging resistance lies in the
polymer comprising 3M™ VHB™ Tapes. The chemical bonds that make up
the polymer chains consist of carbon-carbon single bonds that are highly
resistant to energy in the form of heat or ultraviolet light, as well as
chemical attack. In less durable foams or adhesives, such conditions could
lead to cleaving of the polymer backbone and thus a weakening of
mechanical properties. In the case of acrylic adhesives and foams,
however, additional crosslinking is chemically favored over chain scission
(cleavage). This means that, rather than undergoing a process of
decomposition, the acrylate materials will tend to build modulus very
slightly over extended exposures. This translates to a stronger, long lasting
bond.
Temperature Exposure
Because of the demanding and diverse applications users have for
3M™ VHB™ Tapes, durability has always been a key interest in the
performance of these products. One of the first issues for tapes is
retention of tack and adhesion after exposure to elevated
temperatures. Bonds made with 3M™ VHB™ Tapes can tolerate
periodic, short- term exposures to temperatures up to 300°F (150°C)
for most Foam Tapes.
Composition
Durability Testing
Recommended books on embedded development (Part 23) --- Detailed examples of embedded hardware system design and development
[align=center][size=5]Recommendations for high-quality books on embedded development (Twenty-three) ---[color=#000][backcolor=rgb(237, 235, 235)][font=微软雅黑]Detailed explanation of embedded hardware sy...
tiankai001 Download Centre
Recruitment of part-time
SMS sending and receiving ShenDa PDA sends short messages, and the server receives the mobile Windows Mobile system using the public network, the server receives, two programs contact QQ 412925762...
jimmyyuyu Embedded System
MSP430 IO port input high level sampling problem? ?
Please help me, friends! ! As the title says, an IO port is used as input, initially at a low level, and receives a high level signal. 100 points are sampled relative to this high level. If all 100 po...
neal9431 Microcontroller MCU
【KW41Z】Construction safety monitoring system
Due to the urgency of another project in recent months, the test of KW41 was mainly arranged for several idle brothers in the company. I could only take a look and test occasionally, so I didn't repor...
wforest68 NXP MCU
Stm32 TIM4_CH1
[color=red]stm32 PD12 outputs PWM wave, using TIM4_CH2, PB6 port can output, but PB12, TIM4_CH1 can't, port multiplexing can't work, I don't know what's going on, help me[/color] #include"stm32f10x.h"...
ranxiaoyi stm32/stm8
Discussion on STM32 DMA applied to UART data reception
STM32's UART does not have FIFO. When the communication speed is high, the overhead of not using DMA is too high (LM3S has a 16-level deep FIFO that can trigger an interrupt when it is 7/8 full, with ...
xg_qing stm32/stm8

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Robot
development
community

Index Files: 347  416  1246  1890  2596  7  9  26  39  53 
Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2026 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号